Bond Strength Stability of Self-adhesive Resin Cement to Etched Vitrified Yttria-stabilized Tetragonal Zirconia Polycrystal Ceramic After Thermomechanical Cycling

Maroun, E V ; Guimarães, Jga ; de Miranda, Jr, W G ; Netto, Lrc ; Elias, A B ; da Silva, E M

Operative dentistry, 2019-09, Vol.44 (5), p.545-555 [Periódico revisado por pares]

United States

Texto completo disponível

Citações Citado por
  • Título:
    Bond Strength Stability of Self-adhesive Resin Cement to Etched Vitrified Yttria-stabilized Tetragonal Zirconia Polycrystal Ceramic After Thermomechanical Cycling
  • Autor: Maroun, E V ; Guimarães, Jga ; de Miranda, Jr, W G ; Netto, Lrc ; Elias, A B ; da Silva, E M
  • Assuntos: Dentistry
  • É parte de: Operative dentistry, 2019-09, Vol.44 (5), p.545-555
  • Notas: ObjectType-Article-1
    SourceType-Scholarly Journals-1
    ObjectType-Feature-2
    content type line 23
  • Descrição: The purpose of this study was to evaluate the influence of thermomechanical cycling on the bond strength stability of self-adhesive resin cement to vitrified yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) ceramic. Y-TZP ceramic blocks were divided into four groups according to the surface treatments: AS, as sintered; SB, sandblasted with 50-μm Al O particles; LG, vitrification with a low-fusing glaze and etching with 10% hydrofluoric acid; and HC, vitrification with a ceramic liner and etching with 10% hydrofluoric acid. Lithium disilicate ceramic blocks etched with 10% hydrofluoric acid for 20 seconds (EM) were also tested. Blocks of resin composite were cemented on the ceramic block surfaces using a self-adhesive resin cement. Half of the blocks from each group were cut into beams and submitted to microtensile bond strength (μTBS) testing after immersion in water at 37°C for 24 hours and the other half after mechanical (1,200,000 cycles, 98 N, 2.5 Hz) and thermal (10,000 cycles, 5-55°C, 30-second dwell time) cycling (TMC). Data were analyzed using one-way analysis of variance, Tukey's honest significant difference post hoc test, and Student -test (α=0.05). After 24 hours, EM and LG presented similar and the highest μTBS, whereas AS showed the lowest μTBS ( <0.05). After TMC, EM presented the highest μTBS, followed by LG ( <0.05). Only EM and LG maintained the stability of μTBS after TMC ( >0.05). The bonding to Y-TZP ceramic vitrified with a low-fusing glaze withstood thermomechanical cycling.